Analysis of toughening of magnesia partially stabilized zirconia, due to dilatational transformation

Acta Metallurgica et Materialia - Tập 40 - Trang 1421-1432 - 1992
H. Okada1, T. Tamura1, N. Ramakrishnan1, S.N. Atluri1, J.S. Epstein2
1Computational Modeling and Infrastructure Rehabilitation Center, Georgia Institute of Technology, Atlanta, GA 30332-0356 U.S.A.
2Fracture Behavior Group, Idaho National Engineering Laboratory, P.O. Box 1625, Idaho Falls, ID 83415-2218, U.S.A.

Tài liệu tham khảo

Becher, 1986, Acta metall., 34, 1885, 10.1016/0001-6160(86)90246-4 Evans, 1986, Acta metall., 34, 761, 10.1016/0001-6160(86)90052-0 Budiansky, 1983, Int. J. Solids Struct., 19, 337, 10.1016/0020-7683(83)90031-8 McMeeking, 1982, J. Am. Ceram. Soc., 65, 242, 10.1111/j.1151-2916.1982.tb10426.x Marshall, 1986, J. Am. Ceram. Soc., 69, 173, 10.1111/j.1151-2916.1986.tb07402.x Cox, 1988, J. Engng Mater. Technol., 110, 105, 10.1115/1.3226015 Swain, 1985, J. Am. Ceram. Soc., 68, C, 10.1111/j.1151-2916.1985.tb15305.x Owen, 1980 K. E. Perry, G. May, J. S. Epstein and H. Okada. To be published. Lanteri, 1986, J. Am. Ceram. Soc., 69, 564, 10.1111/j.1151-2916.1986.tb04793.x Wu, 1966, Int. J. Solids Struct., 2, 1, 10.1016/0020-7683(66)90002-3 Ramakrishnan, 1991, Acta metall., 39, 1297, 10.1016/0956-7151(91)90218-P Mura, 1982 Eshelby, 1957, 241, 376 Dravid, 1988, J. Am. Ceram. Soc., 71, C, 10.1111/j.1151-2916.1988.tb05883.x Lambropoulos, 1986, Int. J. Solids Struct., 22, 1083, 10.1016/0020-7683(86)90019-3 Lambropoulos, 1987, 217 Amazigo, 1988, Int. J. Solids, Struct., 24, 751, 10.1016/0020-7683(88)90021-2 Stump, 1988 Rice, 1968, J. appl. Mech., 35, 379, 10.1115/1.3601206 Atluri, 1986 Nielsen (U.S.A.) Inc., Technical data of Nilsen's PSZ. Mori, 1988, J. Am. Ceram. Soc., 71, C, 10.1111/j.1151-2916.1988.tb05929.x Dadkhah, 1990