A combined CP theory and TCD for predicting fatigue lifetime in single-crystal superalloy plates with film cooling holes
Tóm tắt
Từ khóa
Tài liệu tham khảo
Qiu, 2016, Effects of secondary orientation on crack closure behavior of nickel-based single crystal superalloys, Int J Fatigue, 83, 335, 10.1016/j.ijfatigue.2015.11.004
Sabnis, 2016, Microdamage modelling of crack initiation and propagation in FCC single crystals under complex loading conditions, Comput Method Appl M, 312, 468, 10.1016/j.cma.2016.04.018
Pei, 2017, Long-term oxidation behavior and mechanism of DD6 Ni-based single crystal superalloy at 1050 °C and 1100 °C in air, J Alloy Compd, 704, 218, 10.1016/j.jallcom.2017.02.031
Miehe, 2014, Variational gradient plasticity at finite strains. Part III: local–global updates and regularization techniques in multiplicative plasticity for single crystals, Comput Method Appl M, 268, 735, 10.1016/j.cma.2013.08.022
He, 2017, Investigations of film cooling and heat transfer on a turbine blade squealer tip, Appl Therm Eng, 110, 630, 10.1016/j.applthermaleng.2016.08.173
Sahu, 2016, Investigation of the effect of air film blade cooling on thermoeconomics of gas turbine based power plant cycle, Energy, 115, 1320, 10.1016/j.energy.2016.09.069
Li, 2017, A multi-scale crystal plasticity model for cyclic plasticity and low-cycle fatigue in a precipitate-strengthened steel at elevated temperature, J Mech Phys Solids, 101, 44, 10.1016/j.jmps.2016.12.010
Lu, 2017, Constitutive model of 42CrMo steel under a wide range of strain rates based on crystal plasticity theory, Mat Sci Eng A-Struct, 679, 215, 10.1016/j.msea.2016.09.117
Knight, 2016, Crystal plasticity modeling of damage accumulation in dissimilar Mg alloy bi-crystals under high-cycle fatigue, Int J Fatigue, 90, 99, 10.1016/j.ijfatigue.2016.04.009
Knezevic, 2016, A numerical procedure enabling accurate descriptions of strain rate-sensitive flow of polycrystals within crystal visco-plasticity theory, Comput Method Appl M, 308, 468, 10.1016/j.cma.2016.05.025
Ghosh, 2013, Homogenized constitutive and fatigue nucleation models from crystal plasticity FE simulations of Ti alloys, Part 1: macroscopic anisotropic yield function, Int J Plasticity, 47, 182, 10.1016/j.ijplas.2012.12.008
Kirane, 2008, A cold dwell fatigue crack nucleation criterion for polycrystalline Ti-6242 using grain-level crystal plasticity FE model, Int J Fatigue, 30, 2127, 10.1016/j.ijfatigue.2008.05.026
Klusemann, 2014, Microstructural pattern formation in finite-deformation single-slip crystal plasticity under cyclic loading: relaxation vs. gradient plasticity, Comput Method Appl M, 278, 765, 10.1016/j.cma.2014.05.015
Hill, 1966, Generalized constitutive relations for incremental deformation of metal crystals by multislip, J Mech Phys Solids, 14, 95, 10.1016/0022-5096(66)90040-8
Hill, 1972, Constitutive analysis of elastic-plastic crystals at arbitrary strain, J Mech Phys Solids, 20, 401, 10.1016/0022-5096(72)90017-8
Asaro, 1983, Micromechanics of crystals and polycrystals, Adv Appl Mech, 23, 1, 10.1016/S0065-2156(08)70242-4
Rice, 1987, Tensile crack tip fields in elastic-ideally plastic crystals, Mech Mater, 6, 317, 10.1016/0167-6636(87)90030-5
Hong, 2011, A comparative study on thermomechanical and low cycle fatigue failures of a single crystal nickel-based superalloy, Int J Fatigue, 33, 1592, 10.1016/j.ijfatigue.2011.07.009
Arakere NK, Swanson G. Effect of crystal orientation on fatigue failure of single crystal nickel base turbine blade superalloys//ASME Turbo Expo 2000: Power for Land, Sea, and Air. American Society of Mechanical Engineers, 2000: V004T01A004-V004T01A004.
Arakere NK. High-temperature fatigue properties of single crystal superalloys in air and hydrogen//ASME Turbo Expo 2001: Power for Land, Sea, and Air. American Society of Mechanical Engineers, 2001: V004T03A061-V004T03A061.
Levkovitch, 2006, Simulation of deformation and lifetime behavior of a fcc single crystal superalloy at high temperature under low-cycle fatigue loading, Int J Fatigue, 28, 1791, 10.1016/j.ijfatigue.2005.12.006
Levkovitch, 2005, Simulation of fatigue crack propagation in ductile metals by blunting and re-sharpening, Int J Fract, 136, 207, 10.1007/s10704-005-6024-y
Han, 2016, In-situ SEM observation and crystal plasticity finite element simulation of fretting fatigue crack formation in Ni-base single-crystal superalloys, Tribol Int, 101, 33, 10.1016/j.triboint.2016.03.025
Grilli, 2015, Crystal plasticity finite element modelling of low cycle fatigue in fcc metals, J Mech Phys Solids, 84, 424, 10.1016/j.jmps.2015.08.007
Zhang, 2015, Micromechanics based fatigue life prediction of a polycrystalline metal applying crystal plasticity, Mech Mater, 85, 16, 10.1016/j.mechmat.2015.01.020
Yang, 2013, Properties and life prediction of low cycle fatigue behavior on notched DS Ni-based superalloy, Acta Aeronautica et Astronautica Sinica, 34, 1596
Taylor, 2011, Applications of the theory of critical distances in failure analysis, Eng Fail Anal, 18, 543, 10.1016/j.engfailanal.2010.07.002
Leidermark, 2011, A combined critical plane and critical distance approach for predicting fatigue crack initiation in notched single-crystal superalloy components, Int J Fatigue, 33, 1351, 10.1016/j.ijfatigue.2011.05.009
Li, 2016, Assessing the integrity of steel structural components with stress raisers using the Theory of Critical Distances, Eng Fail Anal, 70, 73, 10.1016/j.engfailanal.2016.07.007
Benedetti, 2016, On the combination of the critical distance theory with a multiaxial fatigue criterion for predicting the fatigue strength of notched and plain shot-peened parts, Int J Fatigue, 93, 133, 10.1016/j.ijfatigue.2016.08.015
Louks, 2016, A generalised approach to rapid finite element design of notched materials against static loading using the Theory of Critical Distances, Mater Des, 108, 769, 10.1016/j.matdes.2016.07.047
Natsu, 2008, Research on generation of three-dimensional surface with micro-electrolyte jet machining, CIRP J Manuf Sci Technol, 1, 27, 10.1016/j.cirpj.2008.06.006
Sen, 2005, Analysis of hole quality characteristics in the electro jet drilling process, Int J Mach Tool Manu, 45, 1706, 10.1016/j.ijmachtools.2005.03.005
Taylor, 1938, Plastic strain in metals, J Inst Met, 62, 307
Taylor, 1923, The distortion of an aluminum crystal during a tensile test, Proc R Soc London, 102A, 643
Taylor, 1925, The plastic extension of fracture of aluminum crystal, Proc R Soc London, 108A, 28
Taylor, 1934, The mechanism of plastic deformation of crystal. Part I. Theoretical, Proc R Soc London, 145A, 362
Schmid E. Plasticity of crystal; 1935.
Rice, 1971, Inelastic constitutive relations for solids: an internal-variable theory and its application to metal plasticity, J Mech Phys Solids, 19, 433, 10.1016/0022-5096(71)90010-X
Asaro, 1977, Strain localization in ductile single crystal, J Mech Phys Solids, 25, 309, 10.1016/0022-5096(77)90001-1
Peirce, 1982, An analysis of nonuniform and localized deformation in ductile single crystals, Acta Metall Sin, 30, 1087, 10.1016/0001-6160(82)90005-0
Peirce, 1983, Material rate dependence and localized deformation in crystalline solids, Acta Metall Sin, 31, 1951, 10.1016/0001-6160(83)90014-7
Wu, 1991, Latent hardening in single crystals I, Theory and experiments, Proc R Soc London A: Math, Phys Eng Sci, R Soc, 435, 1, 10.1098/rspa.1991.0127
Bassani, 1991, Latent hardening in single crystals II, analytical characterization and predictions, Proc R Soc London A: Math, Phys Eng Sci, R Soc, 435, 21, 10.1098/rspa.1991.0128
Susmel, 2008, The theory of critical distances to predict static strength of notched brittle components subjected to mixed-mode loading, Eng Fract Mech, 75, 534, 10.1016/j.engfracmech.2007.03.035
Susmel, 2008, On the use of the Theory of Critical Distances to predict static failures in ductile metallic materials containing different geometrical features, Eng Fract Mech, 75, 4410, 10.1016/j.engfracmech.2008.04.018
Susmel, 2013, The Theory of Critical Distances to estimate finite lifetime of notched components subjected to constant and variable amplitude torsional loading, Eng Fract Mech, 98, 64, 10.1016/j.engfracmech.2012.12.007
Yang, 2013, Experimental investigation and life prediction of low cycle fatigue-behavior on notched DS Ni-based superalloy, Acta Aeronautica et Astronautica Sinica, 34, 1596