Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate

Journal of Prosthodontic Research - Tập 56 - Trang 93-101 - 2012
Gerd Göstemeyer1, Michael Jendras2, Lothar Borchers3, Friedrich-Wilhelm Bach2, Meike Stiesch3, Philipp Kohorst3
1Charité Berlin, Department of Operative Dentistry and Periodontology, Assmanshauser Str. 4-6, 14197 Berlin, Germany
2Leibniz University Hannover, Institute of Materials Science, An der Universität 2, 30823 Garbsen, Germany
3Hannover Medical School, Department of Prosthetic Dentistry and Biomedical Materials Science, Carl-Neuberg-Str. 1, 30625 Hannover, Germany

Tài liệu tham khảo

Denry, 2008, State of the art of zirconia for dental applications, Dent Mater, 24, 299, 10.1016/j.dental.2007.05.007 Manicone, 2007, An overview of zirconia ceramics: basic properties and clinical applications, J Dent, 35, 819, 10.1016/j.jdent.2007.07.008 Conrad, 2007, Current ceramic materials and systems with clinical recommendations: a systematic review, J Prosthet Dent, 98, 389, 10.1016/S0022-3913(07)60124-3 Vult von Steyern, 2005, All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study, J Oral Rehabil, 32, 180, 10.1111/j.1365-2842.2004.01437.x Sailer, 2007, A systematic review of the survival and complication rates of all-ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II. Fixed dental prostheses, Clin Oral Implants Res, 18, 86, 10.1111/j.1600-0501.2007.01468.x Kerschbaum, 2009, Complications with Cercon restorations in the first five years in situ, Dtsch Zahnarztl Z, 64, 81 Fischer, 2008, Flexural strength of veneering ceramics for zirconia, J Dent, 36, 316, 10.1016/j.jdent.2008.01.017 Fischer, 2009, Impact of thermal properties of veneering ceramics on the fracture load of layered Ce-TZP/A nanocomposite frameworks, Dent Mater, 25, 326, 10.1016/j.dental.2008.08.001 DeHoff, 2008, Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries, Dent Mater, 24, 744, 10.1016/j.dental.2007.08.008 Fischer, 2009, Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites, Dent Mater, 25, 419, 10.1016/j.dental.2008.09.003 Lenz, 1998, Thermal stresses in metal–ceramic specimens for the ISO crack initiation test (three-point flexure bond test), Dent Mater, 14, 277, 10.1016/S0109-5641(98)00039-6 Bagby, 1990, Metal ceramic compatibility: a review of the literature, J Prosthet Dent, 63, 21, 10.1016/0022-3913(90)90259-F Aboushelib, 2008, Prestresses in bilayered all-ceramic restorations, J Biomed Mater Res B Appl Biomater, 87, 139, 10.1002/jbm.b.31083 Aboushelib, 2006, Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II. Zirconia veneering ceramics, Dent Mater, 22, 857, 10.1016/j.dental.2005.11.014 Fischer, 2007, Effect of thermal misfit between different veneering ceramics and zirconia frameworks on in vitro fracture load of single crowns, Dent Mater J, 26, 766, 10.4012/dmj.26.766 Dundar, 2007, Comparison of two bond strength testing methodologies for bilayered all-ceramics, Dent Mater, 23, 630, 10.1016/j.dental.2006.05.004 1999 Al-Dohan, 2004, Shear strength of core–veneer interface in bi-layered ceramics, J Prosthet Dent, 91, 349, 10.1016/j.prosdent.2004.02.009 Charalambides, 1989, A test specimen for determining the fracture resistance of bimaterial interfaces, J Appl Mech, 56, 77, 10.1115/1.3176069 Suansuwan, 1999, New approach for evaluating metal-porcelain interfacial bonding, Int J Prosthodont, 12, 547 Tholey, 2007, Influence of the bonder on the adhesion of porcelain to machined titanium as determined by the strain energy release rate, Dent Mater, 23, 822, 10.1016/j.dental.2006.06.022 Homann, 2006, Influence of water, loading rate and bonder on the adhesion of porcelain to titanium, J Dent, 34, 485, 10.1016/j.jdent.2005.11.004 Göstemeyer, 2010, Influence of cooling rate on zirconia/veneer interfacial adhesion, Acta Biomater, 6, 4532, 10.1016/j.actbio.2010.06.026 Tholey, 2007, Bonding mechanisms in layered systems for dental use, Quintessenz Zahntech, 33, 160 Swain, 2009, Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures, Acta Biomater, 5, 1668, 10.1016/j.actbio.2008.12.016 Timoshenko, 1925, Analysis of bimetal thermostats, J Opt Soc Am, 11, 233, 10.1364/JOSA.11.000233 Lawn, 1993 2008 O’Brian, 2002 2008 2008 Anusavice, 2007, Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic-based dental prostheses?, Clin Oral Implants Res, 18, 218, 10.1111/j.1600-0501.2007.01460.x Aboushelib, 2009, Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach, Dent Mater, 25, 383, 10.1016/j.dental.2008.09.001 Hsueh, 2008, Analyses of layer-thickness effects in bilayered dental ceramics subjected to thermal stresses and ring-on-ring tests, Dent Mater, 24, 9, 10.1016/j.dental.2006.12.009 Taskonak, 2005, Residual stresses in bilayer dental ceramics, Biomaterials, 26, 3235, 10.1016/j.biomaterials.2004.08.025 DeHoff, 2004, Creep functions of dental ceramics measured in a beam-bending viscometer, Dent Mater, 20, 297, 10.1016/S0109-5641(03)00107-6 Ashkanani, 2008, Flexural and shear strengths of ZrO2 and a high-noble alloy bonded to their corresponding porcelains, J Prosthet Dent, 100, 274, 10.1016/S0022-3913(08)60206-1 Guess, 2008, Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling, Dent Mater, 24, 1556, 10.1016/j.dental.2008.03.028