Cytotoxicity of monomers, plasticizer and degradation by-products released from dental hard chairside reline resins
Tài liệu tham khảo
Dahl, 2006, In vitro biocompatibility of denture relining materials, Gerodontology, 23, 17, 10.1111/j.1741-2358.2006.00103.x
Sofou, 2005, HPLC determination of residual monomers released from heat-cured acrylic resins, Anal Bioanal Chem, 381, 1336, 10.1007/s00216-005-3059-x
Kedjarune, 1999, Release of methyl methacrylate from heat-cured and autopolymerized resins: cytotoxicity testing related to residual monomer, Aust Dent J, 44, 25, 10.1111/j.1834-7819.1999.tb00532.x
Urban, 2007, Residual monomer of reline acrylic resins. Effect of water-bath and microwave post-polymerization treatments, Dent Mater, 23, 363, 10.1016/j.dental.2006.01.021
Lygre, 1995, Leaching from denture base materials in vitro, Acta Odontol Scand, 53, 75, 10.3109/00016359509005950
Lefebvre, 1994, Biocompatibility of visible light-cured resin systems in prosthodontics, J Prosthet Dent, 71, 178, 10.1016/0022-3913(94)90028-0
Lai, 2004, Cytotoxic effects of dental resin liquids on primary gingival fibroblasts and periodontal ligament cells in vitro, J Oral Rehabil, 31, 1165, 10.1111/j.1365-2842.2004.01355.x
Campanha, 2006, Cytotoxicity of hard chairside reline resins: effect of microwave irradiation and water bath postpolymerization treatments, Int J Prosthodont, 19, 195
Jorge, 2007, Biocompatibility of denture base acrylic resins evaluated in culture of L929 cells. Effect of polymerisation cycle and post-polymerisation treatments, Gerodontology, 24, 52, 10.1111/j.1741-2358.2007.00146.x
Weaver, 1980, Reactions to acrylic resin dental prostheses, J Prosthet Dent, 43, 138, 10.1016/0022-3913(80)90176-6
Ali, 1986, The burning mouth sensation related to the wearing of acrylic dentures: an investigation, Br Dent J, 161, 444, 10.1038/sj.bdj.4806008
Lunder, 2000, Chronic urticaria from an acrylic dental prosthesis, Contact Dermatitis, 43, 232
Bohnenkamp, 1996, Traumatic stomatitis following an intraoral denture reline: a clinical report, J Prosthet Dent, 72, 113, 10.1016/S0022-3913(96)90292-9
Barron, 1993, Biocompatibility of visible light-polymerized denture base resins, Int J Prosthodont, 6, 495
Hashimoto, 2000, Estrogenic activity of chemicals for dental and similar use in vitro, J Mater Sci, 11, 465
Jobling, 1995, A variety of environmentally persistent chemicals, including some phthalate plasticizers, are weakly estrogenic, Environ Health Perspect, 103, 582, 10.1289/ehp.95103582
Kim, 2002, Effect of dibutyl phthalate and monobutyl phthalate on cytotoxicity and differentiation in cultured rat embryonic limb bud cells; protection by antioxidants, J Toxicol Environ Health A, 65, 461, 10.1080/15287390252808118
Xiang-Rong, 2007, Kinetics of n-butyl benzyl phthalate degradation by a pure bacterial culture from the mangrove sediment, J Hazard Mater, 140, 194, 10.1016/j.jhazmat.2006.06.054
Seiss, 2007, Identification of 2,3-epoxymethacrylic acid as an intermediate in the metabolism of dental materials in human liver microsomes, Dent Mater, 23, 9, 10.1016/j.dental.2005.11.038
Emmler, 2008, Cytotoxicity of dental composite TEGMA and selected metabolic by-products in human pulmonary cells, Dent Mater, 24, 1670, 10.1016/j.dental.2008.04.001
Koda, 1990, Leachability of denture base acrylic resins in artificial saliva, Dent Mater, 6, 13, 10.1016/0109-5641(90)90037-F
Babich, 1996, Benzoyl peroxide cytotoxicity evaluated in vitro with the human keratinocyte cell line RHEK-1, Toxicology, 106, 187, 10.1016/0300-483X(95)03189-M
Datar, 2004, Effects of subtoxic concentrations of benzoyl peroxide on cell lipid metabolism, J Biomed Mater Res, 71, 685, 10.1002/jbm.a.30207
Urban, 2007
Urban, 2009, Effect of water-bath post-polymerization on the mechanical properties, degree of conversion, and leaching of residual compounds of hard chairside reline resins, Dent Mater, 25, 662, 10.1016/j.dental.2008.10.017
Thonemann, 2002, Responses of L929 mouse fibroblasts, primary and immortalized bovine dental papilla-derived cell lines to dental resin components, Dent Mater, 18, 318, 10.1016/S0109-5641(01)00056-2
Wataha, 1994, Effect of cell line on in vitro metal ion cytotoxicity, Dent Mater, 10, 156, 10.1016/0109-5641(94)90025-6
International Standards Organization, 1999
Tang, 1999, Cytotoxicity tests of in situ polymerized resins: methodological comparisons and introduction of a tissue culture insert as a testing device, J Biomed Mater Res, 45, 214, 10.1002/(SICI)1097-4636(19990605)45:3<214::AID-JBM9>3.0.CO;2-Y
Mosmann, 1983, Rapid colorimetric assay for cellular growth and survival: application to proliferation and cytotoxicity assays, J Immunol Method, 65, 55, 10.1016/0022-1759(83)90303-4
Wataha, 1991, The in vitro effects of metal cations on eukaryotic cell metabolism, J Biomed Mater Res, 25, 1133, 10.1002/jbm.820250907
Yoshii, 1997, Cytotoxic effects of acrylates and methacrylates: relationships of monomer structures and cytotoxicity, J Biomed Mater Res, 37, 517, 10.1002/(SICI)1097-4636(19971215)37:4<517::AID-JBM10>3.0.CO;2-5
Imazato, 2009, Effects of monomers eluted from dental resin restoratives on osteoblast-like cells, J Biomed Mater Res B: Appl Biomater, 88, 378, 10.1002/jbm.b.31067
Sun, 1997, Effects of metal ions on osteoblast-like cell metabolism and differentiation, J Biomed Mater Res, 34, 29, 10.1002/(SICI)1097-4636(199701)34:1<29::AID-JBM5>3.0.CO;2-P
Meier, 2001, Reactive oxygen intermediates involved in cellular regulation, Protoplasma, 217, 101, 10.1007/BF01289419
Geurtsen, 1998, Cytotoxicity of 35 dental resin composite monomers/additives in permanent 3T3 and three human primary fibroblast cultures, J Biomed Mater Res, 41, 474, 10.1002/(SICI)1097-4636(19980905)41:3<474::AID-JBM18>3.0.CO;2-I
Wataha, 1992, Precision of and new methods for testing in vitro alloy cytotoxicity, Dent Mater, 8, 65, 10.1016/0109-5641(92)90056-I
Fujisawa, 1988, 1H and 13C NMR studies of the interaction of eugenol, phenol, and triethyleneglycol dimethacrylate with phospholipid liposomes as a model system for odontoblast membranes, J Dent Res, 67, 1438, 10.1177/00220345880670111501
Silikas, 2000, High pressure liquid chromatography of dentin primers and bonding agents, Dent Mater, 16, 81, 10.1016/S0109-5641(99)00095-0
Atsumi, 2006, (Meth)acrylate monomer-induced cytotoxicity and intracellular Ca(2+) mobilization in human salivary gland carcinoma cells and human gingival fibroblast cells related to monomer hydrophobicity, Biomaterials, 27, 5794, 10.1016/j.biomaterials.2006.07.041
Urban, 2006, Development and application of methods for determination of residual monomer in dental acrylic resins using high performance liquid chromatography, Biomed Chromatogr, 20, 369, 10.1002/bmc.575
Mainwaring, 2001, Methyl methacrylate toxicity in rat nasal epithelium: studies of the mechanism of action and comparisons between species, Toxicology, 158, 109, 10.1016/S0300-483X(00)00332-2
Schwengberg, 2005, In vitro embryotoxicity assessment with dental restorative materials, J Dent, 33, 49, 10.1016/j.jdent.2004.08.001
De Groot, 2001, In vitro biocompatibility of biodegradable dextran-based hydrogels tested with human fibroblasts, Biomaterials, 22, 1197, 10.1016/S0142-9612(00)00266-0
Henriques, 1997, Extrusion of benzoic acid in Saccharomyces cerevisiae by an energy-dependent mechanism, Microbiology, 143, 1877, 10.1099/00221287-143-6-1877
Swauger, 1991, Role of the benzoyloxyl radical in DNA damage mediated by benzoyl peroxide, Chem Res Toxicol, 4, 223, 10.1021/tx00020a016
Milan, 1983, Inhibitors of poly(adenosine diphosphate–ribose) synthesis: effect on other metabolic processes, Science, 223, 589, 10.1126/science.6420886