On the relationship between pore structure and charge passed from RCPT in mineral-free cement-based materials

Materials Chemistry and Physics - Tập 93 - Trang 202-207 - 2005
C.C. Yang1, C.T. Chiang1,2
1Institute of Materials Engineering, National Taiwan Ocean University, Keelung, Taiwan, ROC
2Department of Civil Engineering, Cheng Shiu University, Kaohsiung County, Taiwan, ROC

Tài liệu tham khảo

Kumar, 2003, Cem. Concr. Res., 33, 155, 10.1016/S0008-8846(02)00942-0 Samaha, 1992, ACI Mater. J., 89, 1416 Mehta, 1993 Ngala, 1995, Cem. Concr. Res., 25, 819, 10.1016/0008-8846(95)00072-K Uchikawa, 1996, Cem. Concr. Res., 26, 101, 10.1016/0008-8846(95)00193-X Shi, 1996, Cem. Concr. Res., 26, 1789, 10.1016/S0008-8846(96)00174-3 Jiang, 1999, Cem. Concr. Res., 29, 631, 10.1016/S0008-8846(99)00034-4 Pandey, 2000, Cem. Concr. Res., 30, 19, 10.1016/S0008-8846(99)00180-5 Frias, 2000, Cem. Concr. Res., 30, 561, 10.1016/S0008-8846(00)00203-9 Matusinovic, 2003, Cem. Concr. Res., 33, 1801, 10.1016/S0008-8846(03)00201-1 Ngala, 1997, Cem. Concr. Res., 27, 995, 10.1016/S0008-8846(97)00102-6 Standard test method for electrical indication of concrete's ability to resist chloride ion penetration, ASTM C 1202-97, ASTM, USA, 1994. Standard method of test for rapid determination of the chloride permeability of concrete, AASHTO T277-96, AASHTO, USA, 1996. Whiting, 1981, Public Roads, 45, 101 Li, 1986, Cem. Concr. Res., 16, 749, 10.1016/0008-8846(86)90049-9 Wee, 2000, ACI Mater. J., 97, 221 Yang, 2002, Cem. Concr. Res., 32, 1559, 10.1016/S0008-8846(02)00832-3 Aldea, 2000, Cem. Concr. Res., 30, 465, 10.1016/S0008-8846(00)00200-3 Shane, 1999, Concr. Sci. Eng., 1, 110 Kumar, 2003, Cem. Concr. Res., 33, 417, 10.1016/S0008-8846(02)00974-2 MacMullin, 1956, AIChE J., 2, 393, 10.1002/aic.690020320 Tumidajski, 1996, Cem. Concr. Res., 26, 539, 10.1016/0008-8846(96)00017-8 Beaudoin, 1994, Adv. Cem. Bas. Mater., 1, 224, 10.1016/1065-7355(94)90028-0 Parrott, 1992, Cem. Concr. Res., 22, 1077, 10.1016/0008-8846(92)90038-W