Evolution of ferroelectric LiNbO3 phase in a reactive glass matrix (LiBO2–Nb2O5)

Journal of Non-Crystalline Solids - Tập 351 - Trang 1455-1465 - 2005
N. Syam Prasad1, K.B.R. Varma2
1Materials Research Centre, Indian Institute of Science, Bangalore 560 012, India
2Materials Research Centre, Indian Institute of Science, Bangalore-560 012, India

Tài liệu tham khảo

Borrelli, 1967, J. Appl. Phys., 38, 4243, 10.1063/1.1709111 Glass, 1977, Appl. Phys. Lett., 31, 249, 10.1063/1.89670 Komatsu, 1991, J. Non-Cryst. Solids, 135, 105, 10.1016/0022-3093(91)90410-8 Sigaev, 1995, Mater. Sci. Eng. B, 32, 17, 10.1016/0921-5107(94)01167-2 Shyu, 2000, J. Am. Ceram. Soc., 83, 3135, 10.1111/j.1151-2916.2000.tb01694.x Prasad, 2003, J. Solid State Chem., 173, 209, 10.1016/S0022-4596(03)00026-4 Boyd, 1964, Appl. Phys. Lett., 5, 234, 10.1063/1.1723604 Peterson, 1964, Appl. Phys. Lett., 5, 62, 10.1063/1.1754053 Magnusson, 1974, Appl. Opt., 13, 1545, 10.1364/AO.13.1545_1 Abouelleil, 1989, J. Am. Ceram. Soc., 72, 1311, 10.1111/j.1151-2916.1989.tb07644.x Imaoka, 1968, J. Ceram. Soc. Jpn., 76, 160 Nassau, 1979, J. Am. Ceram. Soc., 62, 503, 10.1111/j.1151-2916.1979.tb19116.x Kim, 1993, J. Non-Cryst. Solids, 162, 201, 10.1016/0022-3093(93)90757-O Shankar, 1999, J. Non-Cryst. Solids, 243, 192, 10.1016/S0022-3093(98)00815-1 Hu, 2000, J. Non-Cryst. Solids, 278, 170, 10.1016/S0022-3093(00)00343-4 Todorovic, 1997, Ceram. Int., 23, 55, 10.1016/0272-8842(95)00140-9 JCPDS-International center for diffraction data, 20-0631 JCPDS-International center for diffraction data, 36-0307 Prasad, 2005, J. Am. Ceram. Soc., 88, 357, 10.1111/j.1551-2916.2005.00055.x Kim, 1996, J. Mater. Sci., 31, 2159, 10.1007/BF00356640 Tomozawa, 1977, vol. 12 Murugan, 2002, Ferroelectrics, 266, 259, 10.1080/714939491 Stevels, 1957, Handbuch der physik, 20, 372 Taylor, 1957, J. Soc. Glass Technol., 41, 350T Taylor, 1959, J. Soc. Glass Technol., 43, 124T Charles, 1961, J. Appl. Phys., 32, 1115, 10.1063/1.1736169 Elliott, 1988, Solid State Ionics, 27, 131, 10.1016/0167-2738(88)90003-3 Doi, 1992, Phys. Chem. Glasses, 33, 184 Lanfredi, 1999, J. Appl. Phys., 86, 2215, 10.1063/1.371033 Lewis, 1989 Megaw, 1954, Acta Crystallogr., 7, 187, 10.1107/S0365110X54000527 Cha, 1994, Ferroelectrics Lett., 17, 111, 10.1080/07315179408204272