Combustion synthesis of (TiC + SiC) composite powders by coupling strong and weak exothermic reactions

Journal of Alloys and Compounds - Tập 492 - Trang L82-L86 - 2010
Guanghua Liu1,2, Jiangtao Li1, Kexin Chen2, Heping Zhou2
1Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing, 100190, People’s Republic of China
2Department of Materials Science and Engineering, State Key Laboratory of New Ceramics and Fine Processing, Tsinghua University, Beijing 100084, People's Republic of China

Tài liệu tham khảo

Munir, 1989, Mater. Sci. Rep., 3, 277, 10.1016/0920-2307(89)90001-7 Merzhanov, 1995, Ceram. Int., 21, 371, 10.1016/0272-8842(95)96211-7 Moore, 1995, Prog. Mater. Sci., 39, 243, 10.1016/0079-6425(94)00011-5 Ren, 1998, Ceram. Eng. Sci. Proc., 19, 461, 10.1002/9780470294499.ch54 Feng, 1994, J. Appl. Phys., 76, 1927, 10.1063/1.357677 Dunmead, 1989, J. Am. Ceram. Soc., 72, 2318, 10.1111/j.1151-2916.1989.tb06083.x Yeh, 2005, Ceram. Int., 31, 719, 10.1016/j.ceramint.2004.07.013 Beaufort, 2002, J. Mater. Syn. Proc., 10, 277, 10.1023/A:1023098227041 Han, 2000, Mater. Sci. Eng. A, 280, 328, 10.1016/S0921-5093(99)00606-1 Cochepin, 2007, J. Cryst. Growth, 304, 481, 10.1016/j.jcrysgro.2007.02.018 Maglia, 2004, J. Mater. Sci., 39, 5227, 10.1023/B:JMSC.0000039215.28545.2f Liu, 2009, Int. J. Miner. Metall. Mater., 16, 322, 10.1016/S1674-4799(09)60058-3 Kata, 1997, Solid State Ionics, 101–103, 65 Yin, 1999 Liversage, 2007, J. Am. Ceram. Soc., 90, 2189, 10.1111/j.1551-2916.2007.01666.x Wang, 2004, J. Mater. Sci., 39, 4515, 10.1023/B:JMSC.0000034145.54280.53 Kim, 2000, J. Mater. Sci., 35, 5569, 10.1023/A:1004848828322