Effect of holding time and pressure on properties of ZrB2–SiC composite fabricated by the spark plasma sintering reactive synthesis method

Yuan Zhao1,2, Lian-Jun Wang1, Guo-Jun Zhang1, Wan Jiang1, Li-Dong Chen1
1State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Dingxi Road, Shanghai 200050, China
2Graduate School of Chinese Academy of Sciences, 19 Yuquan Road, Beijing 100049, China

Tài liệu tham khảo

Mroz, 1995, Annual mineral review: zirconium diboride, Am Ceram Soc Bull, 74, 164 Upadhya, 1997, Materials for ultrahigh temperature structural applications, Am Ceram Soc Bull, 72, 51 Fahrenholtz, 2007, Refractory diborides of zirconium and hafnium, J Am Ceram Soc, 90, 1347, 10.1111/j.1551-2916.2007.01583.x Opeka, 2004, Oxidation-based materials selection for 2000°C+ hypersonic aerosurfaces: theoretical consideration and historical experience, J Mater Sci, 39, 5887, 10.1023/B:JMSC.0000041686.21788.77 Fahrenholtz, 2007, Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region, J Am Ceram Soc, 9, 143, 10.1111/j.1551-2916.2006.01329.x Tripp, 1973, Effect of an SiC addition on the oxidation of ZrB2, Ceram Bull, 52, 612 Chamberlain, 2004, High-strength zirconium diboride-based ceramics, J Am Ceram Soc, 87, 1170, 10.1111/j.1551-2916.2004.01170.x Monteverde, 2005, Beneficial effects of an ultra-fine α-SiC incorporation on the sinterability and mechanical properties of ZrB2, Appl Phys A, 82, 329, 10.1007/s00339-005-3327-9 Monteverde, 2005, Development and characterization of metal-diboride-based composites toughened with ultra-fine SiC particulates, Solid State Sci, 7, 622, 10.1016/j.solidstatesciences.2005.02.007 Hwang Sung, 2007, Improved processing and oxidation-resistance of ZrB2 ultrahigh temperature ceramics containing SiC nanodispersoids, Mat Sci Eng A, 464, 216, 10.1016/j.msea.2007.03.002 Zhao, 2007, Preparation and microstructure of a ZrB2–SiC composite fabricated by the spark plasma sintering reactive synthesis (SPS-RS) method, J Am Ceram Soc, 90, 4033 Lee, 2002, Hardness and fracture toughness of pressureless-sintered boron carbide (B4C), J Am Ceram Soc, 85, 1291, 10.1111/j.1151-2916.2002.tb00260.x