Microstructure evolution and tribological properties of TiB2/Ni–Ta cermets

Journal of the European Ceramic Society - Tập 32 Số 9 - Trang 1941-1948 - 2012
Ľuboš Bača1, Zoltán Lenčéš2, Christian Jogl1, Erich Neubauer3, Martin Vitkovič2, A. Merstallinger1, Pavol Šajgalı́k2
1Aerospace & Advanced Composites GmbH, A-2444 Seibersdorf, Austria
2Institute of Inorganic Chemistry, Slovak Academy of Sciences, Dúbravská cesta 9, SK-845 36 Bratislava, Slovakia
3RHP-Technology GmbH & Co. KG, Forschungs- und Technologiezentrum, A-2444 Seibersdorf, Austria

Tóm tắt

Từ khóa


Tài liệu tham khảo

Wang, 2002, Influence of hot pressing sintering temperature and time on microstructure and mechanical properties of TiB2 ceramics, J Eur Ceram Soc, 22, 1045, 10.1016/S0955-2219(01)00424-1

Horlock, 2002, Thermally sprayed Ni(Cr)–TiB2 coatings using powder produced by self-propagating high temperature synthesis: microstructure and abrasive wear behaviour, Mater Sci Eng A, 336, 88, 10.1016/S0921-5093(01)01918-9

Sigl, 1993, Continuous turning with TiB2 cermets: preliminary cutting tests, Int J Refract Met Hard Mater, 12, 95, 10.1016/0263-4368(93)90020-G

Ferber, 1983, Effect of microstructure on the properties of TiB2 ceramics, J Am Ceram Soc, 1, C2

Jaroszewicz, 2006, Preparation of a TiB2 composite with a nickel matrix by pulse plasma sintering with combustion synthesis, J Eur Ceram Soc, 26, 2427, 10.1016/j.jeurceramsoc.2005.05.001

Lide, 2000

Bansal, 2005

Kokabi, 1997, Studies of the Mechanical Properties of TiB2–6%TaB2–1%CoB–x%mZrO2, J Eur Ceram Soc, 17, 885, 10.1016/S0955-2219(96)00189-6

Okamoto, 2000, Ni–Ta (nickel–tantalum), J Phase Equilib, 21, 497, 10.1361/105497100770339798

Murray, 1981, The Ta–Ti (tantalum–titanium) system, Bull Alloy Phase Diagrams, 2, 62, 10.1007/BF02873705

Ansel, 1998, Interdiffusion in the body cubic centered β-phase of Ta–Ti alloys, Acta Mater, 46, 423, 10.1016/S1359-6454(97)00272-3

Suzuki, 2001, Adhesion and abrasion of sputter-deposited ceramic thin films on glass, vol. 2, 235

Yang, 2004, Sliding wear behaviour and tribofilm formation of ceramics at high temperatures, Surf Coat Technol, 184, 270, 10.1016/j.surfcoat.2003.10.157

Ajayi, 1993, Sliding wear of silicon carbide–titanium boride ceramic matrix composites, J Am Ceram Soc, 76, 511, 10.1111/j.1151-2916.1993.tb03815.x

Wäsche, 2004, Tribological performance of SiC and TiB2 against SiC and Al2O3 at low sliding speeds, Wear, 256, 695, 10.1016/S0043-1648(03)00444-7

Ribeiro, 2007, Tribological investigation of tantalum boride coating under dry and simulated body fluid conditions, Wear, 262, 1380, 10.1016/j.wear.2007.01.009

Vleugels, 2002, Unlubricated fretting wear of TiB2-containing composites against bearing steel, Metall Mater Trans A, 33A:, 3847, 10.1007/s11661-002-0257-4

Darabara, 2008, A TiB2 metal matrix composite coating enriched with nitrogen: microstructure and wear properties, Appl Surf Sci, 254, 4144, 10.1016/j.apsusc.2007.12.044