Layered growth of Ti2AlC and Ti3AlC2 in combustion synthesis

Materials Letters - Tập 61 - Trang 779-784 - 2007
Guanghua Liu1, Kexin Chen1, Heping Zhou1, Junming Guo2, Kegang Ren1, J.M.F. Ferreira3
1Department of Materials Science and Engineering, State Key Laboratory of New Ceramics and Fine Processing, Tsinghua University, Beijing 100084, People's Republic of China
2Department of Chemistry, Honghe University, Yunnan, 661100, People's Republic of China
3Department of Ceramics and Glass Engineering, University of Aveiro, CICECO, 3810-193, Aveiro, Portugal

Tài liệu tham khảo

Pietzka, 1994, J. Phase Equilib., 15, 392, 10.1007/BF02647559 Barsoum, 1996, J. Am. Ceram. Soc., 79, 1953, 10.1111/j.1151-2916.1996.tb08018.x Barsoum, 1997, Scr. Metall. Mater., 36, 535, 10.1016/S1359-6462(96)00418-6 Zhou, 2000, Phys. Rev., B, 61, 12570, 10.1103/PhysRevB.61.12570 Rawn, 2000, Mater. Res. Bull., 35, 1785, 10.1016/S0025-5408(00)00383-4 Goto, 1987, Mater. Res. Bull., 22, 1195, 10.1016/0025-5408(87)90128-0 Tzenov, 2000, J. Am. Ceram. Soc., 83, 825, 10.1111/j.1151-2916.2000.tb01281.x Baroum, 1997, Scr. Mater., 36, 535, 10.1016/S1359-6462(96)00418-6 Zhou, 2003, Mater. Sci. Eng., A Struct. Mater.: Prop. Microstruct. Process., 352, 333, 10.1016/S0921-5093(02)00937-1 Lee, 1997, J. Am. Ceram. Soc, 80, 53, 10.1111/j.1151-2916.1997.tb02790.x Zhou, 2001, J. Mater. Sci. Lett., 20, 1971, 10.1023/A:1013147121618 Guo, 2003, Rare Metal Mater. Eng., 32, 1029 Ge, 2003, J. Eur. Ceram. Soc., 23, 567, 10.1016/S0955-2219(02)00098-5 Tang, 2001, J. Cryst. Growth, 222, 130, 10.1016/S0022-0248(00)00870-8 Hartman, 1973