Origin of Deterioration for LiNiO[sub 2] Cathode Material during Storage in Air

The Electrochemical Society - Tập 7 Số 7 - Trang A190 - 2004
Han-san LIU1, Z. R. Zhang1, Zhengliang Gong1, Yong Yang1
1#N#State Key Laboratory for Physical Chemistry of Solid Surfaces and Department of Chemistry, Xiamen University, Xiamen 361005, China #N#

Tóm tắt

Từ khóa


Tài liệu tham khảo

Tarascon, 2001, Nature (London), 414, 361, 10.1038/35104644

Delmas, 1999, Electrochim. Acta, 45, 243, 10.1016/S0013-4686(99)00208-X

Ueda, 1994, J. Electrochem. Soc., 141, 2010, 10.1149/1.2055051

Gao, 1998, Electrochem. Solid-State Lett., 1, 117, 10.1149/1.1390656

D’Epifanio, 2001, Phys. Chem. Chem. Phys., 3, 4399, 10.1039/b104615m

Matsumoto, 1999, J. Power Sources, 81-82, 558, 10.1016/S0378-7753(99)00216-5

Moshtev, 1999, J. Power Sources, 81-82, 434, 10.1016/S0378-7753(99)00247-5

Liu, 2003, J. Solid State Electrochem., 7, 456, 10.1007/s10008-002-0342-z

Liu, 2004, Electrochim. Acta, 49, 1151, 10.1016/j.electacta.2003.11.001

A. C. Larson and R. B. Von Dreele, LANSCE, MS-H805, Los Alamos National Laboratory, Los Alamos, NM.

Galtayries, 1999, J. Electron Spectrosc. Relat. Phenom., 98-99, 267, 10.1016/S0368-2048(98)00292-8

Miyazaki, 1997, Appl. Surf. Sci., 121-122, 492, 10.1016/S0169-4332(97)00347-4

Gottschall, 1998, Inorg. Chem., 37, 1513, 10.1021/ic9709279

Zhao, 1996, Appl. Catal., B, 8, 281, 10.1016/0926-3373(95)00067-4

Iwamoto, 1976, J. Phys. Chem., 80, 1989, 10.1021/j100559a008