Interaction of molten aluminum with porous TiB2-based ceramics containing Ti–Fe additives

Journal of the European Ceramic Society - Tập 32 Số 4 - Trang 937-945 - 2012
Hamed Heidari1, Houshang Alamdari1, D. Dubé1, Robert Schulz2
1Department of Mining, Metallurgical and Materials Engineering, Université Laval, Québec, QC, Canada G1V 0A6
2Hydro-Quebec Research Institute, 1800 Boul. Lionel Boulet, Varennes, QC, Canada J3X 1S1

Tóm tắt

Từ khóa


Tài liệu tham khảo

Hatch, 1984

Sørlie, 1994, Inert and wettable cathodes

Billehaug, 1980, Inert cathodes for aluminum electrolysis in Hall–Heroult cells. Pt. I, Aluminum, 56, 642

Richerson, 1998, Aluminum industry

Basu, 2006, Processing and properties of monolithic TiB2 based materials, Int Mater Rev, 51, 352, 10.1179/174328006X102529

Cutler, 1991, Engineering properties of borides, 787

Barandika, 1999, Consolidation, microstructure, and mechanical properties of a TiB2–Ni3Al composite, Mater Res Bull, 34, 53, 10.1016/S0025-5408(98)00202-5

Baik, 1987, Effect of oxygen contamination on densification of TiB2, J Am Ceram Soc, 70, 527, 10.1111/j.1151-2916.1987.tb05699.x

McMinn, 1992, Review of RHM cathode development

Dorward, 1982, Aluminum penetration and fracture of titanium diboride, J Am Ceram Soc, 65, C-6, 10.1111/j.1151-2916.1982.tb09927.x

Jensen, 2008, Degradation of TiB2 ceramics in liquid aluminum, J Eur Ceram Soc, 28, 3155, 10.1016/j.jeurceramsoc.2008.05.011

Kang, 2001, Pressureless sintering and properties of titanium diboride ceramics containing chromium and iron, J Am Ceram Soc, 84, 893, 10.1111/j.1151-2916.2001.tb00763.x

Pettersen, 1997

Einarsrud, 1997, Pressureless sintering of titanium diboride with nickel, nickel boride, and iron additives, J Am Ceram Soc, 80, 3013, 10.1111/j.1151-2916.1997.tb03227.x

Heidari, 2011, Pressureless sintering of TiB2-based composites using Ti and Fe additives for development of wettable cathodes

Heidari H, Alamdari H, Dubé D, Schulz R. Investigating the potential of TiB2-based composites with Ti and Fe additives as wettable cathode. Mater Sci Forum; in press.

Nord-Varhaug, 1996, TEM investigation of impurity phases and the penetration of liquid aluminum in hot isostatically pressed TiB2 compacts, J Am Ceram Soc, 79, 1147, 10.1111/j.1151-2916.1996.tb08566.x

Rhee, 1970, Wetting of ceramics by liquid aluminum, J Am Ceram Soc, 53, 386, 10.1111/j.1151-2916.1970.tb12138.x

Jones, 1976, Factors affecting the grain-refinement of aluminum using titanium and boron additives, Metall Mater Trans B, 7, 223, 10.1007/BF02654921

Ghosh, 2005, Al–Fe–Ti (Aluminium–Iron–Titanium)

Kattner, 1992, Thermodynamic assessment and calculation of the Ti–Al system, Metall Mater Trans A, 23, 2081, 10.1007/BF02646001

Palm, 2005, Assessment of the Al–Fe–Ti system, Intermetallics, 14, 1291, 10.1016/j.intermet.2005.11.026

Raghavan, 2002, Al–Fe–Ti (aluminum–iron–titanium), J Phase Equilib, 23, 367, 10.1361/105497102770331613

Palm, 1995, The Fe–Al–Ti system, J Phase Equilib, 16, 209, 10.1007/BF02667305

Shahverdi, 2002, Microstructural analysis of interfacial reaction between molten aluminium and solid iron, J Mater Process Tech, 124, 345, 10.1016/S0924-0136(02)00225-X

Grin, 1994, Refinement of the Fe4Al13 structure and its relationship to the quasihomological homeotypical structures, Z Krist-New Cryst St, 209, 479

Yanson, 1995, Crystal structure of Fe4Ti0.93Al12.07, a substitutional variant of the Fe4Al13 structure type, J Alloys Compd, 219, 135, 10.1016/0925-8388(94)05023-6

MacDonald, 1992, Transient liquid phase bonding, Annu Rev Mater Sci, 22, 23, 10.1146/annurev.ms.22.080192.000323

Weirauch, 2005, The wettability of titanium diboride by molten aluminum drops, J Mater Sci, 40, 2301, 10.1007/s10853-005-1949-0